Top
] [
Japanese
]
Minerals transit to other phases by changing condition
Anilite
=>
Digenite
(by powdering)
Aragonite
=>
Calcite
(above 400 degree)
β-Quartz
=>
Tridymite
(above 870 degree)
β-Sulphur
=>
Sulphur
(in some weeks at ambient condition, Unstable below 95.4 degree)
Coesite
=>
Stishovite
(above 10 GPa and above 500 degree)
Feroxyhyte
=>
Goethite
Leadhillite
=>
Susannite
(above 50 degree, Reversible)
Mercury
=> Vapor (at room temperature)
Quartz
=>
β-Quartz
(above 573 degree)
Quartz
=>
Coesite
(2.0-10 GPa and above 500 degree)
Quartz
=>
Stishovite
(above 10 GPa and above 500 degree)
Rosickýite (Rosickyite) =>
Sulphur
(Ambient condition)
Sulphur
=>
β-Sulphur
(above 95.4 degree)
Susannite
=>
Leadhillite
(below 50 degree, Reversible)
Tridymite
=>
Cristobalite
(above 1470 degree)
Vaterite
=>
Aragonite
(in boiling water)
Vaterite
=>
Calcite